brass coated steel fiber construction requirement

1. First put the steel fiber and coarse aggregate into the blender and stir for about 30 seconds, so that the steel fiber is dispersed in the stone without agglomeration

2. Then put the sand and cement into the mixer and dry mix for 30 seconds;

3.Then add water to the rotating mixer, and let the machine stir for about 3 minutes.

4.Steel fibrous concrete build, mix and use at the same time at the same time, water and smash serially, dose sews and can’t get rid of the construction joint and should be shaken closely knit while building less than dividing.

5.Wipe surface, keep line steel fibrous concrete have, collect thick detailed material, sand rate loud, fiber messy to characteristic that is distribute, adopt machinery wipe flat, prevent the fiber from exposing. Adopt device of line kept pigeonhole line craft can also avoid.draw hair produce fiber expose the phenomenon, after 24 hours, according to the maintenance in time of the routine, summer employ idiot, etc. To cover, pay attention to keeping warm in winter.


Post time: Jul-20-2023